Asymmetric surface modification of poly(ethylene terephthalate)
2006-01-13 09:22
浏览:1901次
分享:
资料摘要:
Poly(ethylene terephthalate) (PET) films were treated with CF4 plasma immersion. The samples were processed at different RF powers and treatment time. The surface modification of PET films was evaluated by water contact angle (CA), X-ray photoelectron spectroscopy (XPS) and atomic force microscope (AFM). Decrease in contact angle of both sides of PET films was observed under mild treatment conditions. However, as raising treatment power and/or time, the change in contact angle between the two sides of PET films was different. The relatively hydrophobic and hydrophilic surfaces were being in situ formed on the two sides of PET films, respectively. And the extreme values of water contact angle reached 108.63 and 7.568,
respectively. XPS analyses revealed that there was a substantial incorporation of fluorine and/or oxygen atoms in both side surfaces. The relative chemical composition of the C (ls) spectra’s showed the incorporation of non-polar fluorine-based functionalities (i.e. –CF–CFn–, –CF2– or –CF3 groups) and polar oxygen-based functionalities (i.e. –COOH or –OH groups) in
the surfaces. Correlation between the plasma parameters and the surface modification of PET films is also discussed.
下载本篇资料:
Asymmetric surface modification of poly(ethylene terephthalate)
224KB
推荐资料
Thermofisher Labserv CO150 CO2培养箱,易于操作和维护,为您细胞培养提供了良好的生存环境,并且添加了有效的湿热灭菌功能,是您细胞安心培养的“兵工厂”。
熟悉ALPHA 1-2 LDplus冻干机的使用者都了解,其广泛应用于植物提取物、生物样品、药物制剂研究中的冻干实验。但除了这些典型的应用,仍有一些其他典型实验,也是可以用到ALPHA 1-2 LDplus的。那我们就来看看,还有哪些是我们未知或不熟悉的典型应用:
德国Christ公司是专业生产真空离心浓缩仪的厂家,有着60多年的历史。就其浓缩仪中样品温度的变化,我们进行了详细的数据记录(图1、图2所示),从图1我们发现,当真空值设为7mbar,腔体加热温度设为79℃时,离心腔在61~79℃逐渐升温,对应的转子温度是51.1~71.7℃逐渐升温,而样品温度在14.7~18.2度之间。
离心机是实验室最常用的仪器设备,在任何实验中,离心时的容量需求以及转速表现是使用者最关心的两个方面,那我们就来梳理下常规实验中所需的离心容量及转速情况: