Platinum ditelluride (PtTe2) is a member of transition metal dichalcogenide (TMDCs) family with the MX2 formula. In the bulk form, it is an established metal with complex band structure, in the monolayer it is arguably both semiconductor with band gap value in the far IR or metallic (J. Phys. C: Solid State Phys. 19, 995).
 
As they are semiconductor grade and highly crystalline, you do not need to worry about amorphous phase, defects, or contamination. The crystal size is very large in size and they are perfectly layered in the 001 direction (c-axis - see XRD pattern-) and thus it is very easy to exfoliate and yield monolayers up to 100& yield rate. Single domain size is much larger than 50 microns which enables you to yield large monolayer areas. 
 
The crystals were measured and confirmed by x-ray diffraction (XRD), x-ray photoelectron spectroscopy, Raman, SIMS, and Auger electron spectroscopy techniques. 
 
4 years of growth optimization : In these 4 years, we have perfected our PtTe? growth to fit to your needs. We offer perfect stoichiometry (no other hidden phases), no amorphous regions, superior domain sizes yielding large monolayers, Our crystals have impressive semiconductor purity levels (99.9995 or higher) to bring you highest quality materials at large sizes.
 
Growth method matters> Flux zone or CVT growth method? Contamination of halides and point defects in layered crystals are well known cause for their reduced electronic mobility, poor e-h recombination, low-PL emission, and lower optical absorption. Flux zone technique is a halide free technique used for synthesizing truly semiconductor grade vdW crystals. This method distinguishes itself from chemical vapor transport (CVT) technique in the following regard: CVT is a quick (~2 weeks) growth method but exhibits poor crystalline quality and the defect concentration reaches to 1E11 to 1E12 cm-2 range. In contrast, flux method takes long (~3 months) growth time, but ensures slow crystallization for perfect atomic structuring, and impurity free crystal growth with defect concentration as low as 1E9 - 1E10 cm-2. So if your research needs truly high quality crystals for optoelectronics, scanning tunneling microscopy, spectroscopy, and other projects that rely on defect free crystals, flux zone growth is ideal for you. However, if you need catalytic materials presence of defects typically helps and in such case CVT method is better suited. During check out just state which type of growth process is preferred. Unless otherwise stated, 2Dsemiconductors ships Flux zone crystals as a default choice.


工商信息

企业名称

上海巨纳科技有限公司

企业信息已认证

企业类型

信用代码

310109000501433

成立日期

2009-04-01

注册资本

1000

经营范围

通信设备、光电源、生物科技专业领域内的技术开发、技术转让、技术咨询、技术服务;销售仪器仪表,电子元器件,机械设备及配件,通信设备及相关产品(除卫星地面接收装置),日用百货,从事货物及技术的进出口业务。【企业经营涉及行政许可的,凭许可证件经营】

联系方式
PtTe2 二碲化铂晶体 (Platinum Ditelluride)由上海巨纳科技有限公司为您提供,如您想了解更多关于PtTe2 二碲化铂晶体 (Platinum Ditelluride)价格、规格、特点、分类选择等信息,欢迎咨询厂家。除供应PtTe2 二碲化铂晶体 (Platinum Ditelluride)外,还可为您提供金云母 (10片装)MICA phlogopite 、【巨纳】单层二硫化铼(10x10mm)连续薄膜-衬底可选、铜基石墨烯薄膜(5*5cm) 等耗材,公司有专业的客户服务团队,是您值得信赖的合作伙伴,上海巨纳客服电话。
推荐产品
供应产品
相关品类

上海巨纳科技有限公司

沟通底价

提交后,商家将派代表为您专人服务

获取验证码

{{maxedution}}s后重新发送

获取多家报价,选型效率提升30%
提交留言
点击提交代表您同意 《用户服务协议》 《隐私政策》 且同意关注厂商展位