Our WSSe alloys with the chemical formula WS2xSe2(1-x) crystals perfectly crystallize in 2H phase and come at different alloy ratios x. Our crystals are grown using two different techniques through chemical vapor transport (CVT) or flux zone growth (see description of these two methods below) and their composition values were determined by XPS, SAED, and EDS measurements. These crystals all possess extremely narrow PL bandwidths, display clean PL spectra, high carrier mobility, extremely clean and sharp XRD peaks, and negligible amount of defects (see published results as well as CVT vs. Flux based methods below ). These crystals come with guaranteed alloying and valleytronic response, sharp PL, and good electronic response.

Important advantages of our crystals

1. Crystals come fully characterized using macro, micro, and nanoscale measurements (see below)

2. Thanks to our improved flux zone growth method, our crystals are homogeneously alloyed which means across the specimen you will only find one particular x composition.

3. No separation: Phase separation is commonly observed in 2D TMDCs alloys when cooling profiles are not controlled carefully. Our R&D team has worked over five (5) years to solely solve this problem.

Properties of layered WSSe alloys

Growth method matters> Flux zone or CVT growth method? Contamination of halides and point defects in layered crystals are well known cause for their reduced electronic mobility, reduced anisotropic response, poor e-h recombination, low-PL emission, and lower optical absorption. Flux zone technique is a halide free technique used for synthesizing truly semiconductor grade vdW crystals. This method distinguishes itself from chemical vapor transport (CVT) technique in the following regard: CVT is a quick (~2 weeks) growth method but exhibits poor crystalline quality and the defect concentration reaches to 1E11 to 1E12 cm-2 range. In contrast, flux method takes long (~3 months) growth time, but ensures slow crystallization for perfect atomic structuring, and impurity free crystal growth with defect concentration as low as 1E9 - 1E10 cm-2. During check out just state which type of growth process is preferred. Unless otherwise stated, 2Dsemiconductors ships Flux zone crystals as a default choice.

http://meetings.aps.org/Meeting/MAR18/Session/K36.3

http://meetings.aps.org/Meeting/MAR17/Session/V1.14


WSSe 硒化硫钨晶体 (Tungsten Sulfide Selenide)信息由上海巨纳科技有限公司为您提供,如您想了解更多关于WSSe 硒化硫钨晶体 (Tungsten Sulfide Selenide)报价、型号、参数等信息,欢迎来电或留言咨询。

除供应WSSe 硒化硫钨晶体 (Tungsten Sulfide Selenide)外,上海巨纳科技有限公司还可为您提供Monolayer WS2 Powder 单层二硫化钨粉末Tellurene 碲化物Bi2-xTlxTe3 钛合金-二碲化铋晶体等产品,公司有专业的客户服务团队,是您值得信赖的合作伙伴。