回复luci发表于:2020/1/16 13:08:18悬赏金额:
14积分 状态:
未解决
材料为20CrMnTi,渗碳后淬火,180℃回火。渗层深度约0.6mm,图1约是表层0.2mm处视场,图2是芯部视场。请问,从图中能看出残余奥氏体吗?
[img=,750,562]https://ng1.17img.cn/bbsfiles/images/2016/01/201601161303_582052_2534456_3.jpg[/img]